Sign In | Join Free | My chinacomputerparts.com
China Suzhou Vanforge Metals Co.,  Ltd. logo
Suzhou Vanforge Metals Co., Ltd.
Most sincerity to our customers and employees. To be a highly reliable business partner for our customers. To be a respectable company for creating values for our employees.
Active Member

7 Years

Home > Capillary Coiled Tubing >

Capillary 2507 Super Duplex Capillary Coiled Tubing High Tensile Strength Stress

Suzhou Vanforge Metals Co., Ltd.
Contact Now

Capillary 2507 Super Duplex Capillary Coiled Tubing High Tensile Strength Stress

Capillary 2507 Super Duplex Capillary Coiled Tubing High Tensile Strength Stress

Capillary 2507 Super Duplex Tubing High Tensile Strength Stress Corrosion Super Duplex Stainless 2507, Chemical composition Element Composition, % Chromium 24.0-26.0 Nickel 6.0-8.0 Molybdenum 3.0-5.0 ...

Product Tags:

stainless steel coil tubing

      

seamless hydraulic tubing

      
Send your message to this supplier
 
*From:
*To: Suzhou Vanforge Metals Co., Ltd.
*Subject:
*Message:
Characters Remaining: (0/3000)